Weld Crack in Blaze King Princess

  • Active since 1995, Hearth.com is THE place on the internet for free information and advice about wood stoves, pellet stoves and other energy saving equipment.

    We strive to provide opinions, articles, discussions and history related to Hearth Products and in a more general sense, energy issues.

    We promote the EFFICIENT, RESPONSIBLE, CLEAN and SAFE use of all fuels, whether renewable or fossil.
  • Hope everyone has a wonderful and warm Thanksgiving!

mdmallard

Member
Hearth Supporter
Nov 20, 2014
16
Maryland
I discovered a 3" long crack in a weld on my Blaze King Princess at the end of burning season (March, 2023). I called my dealer who installed it and they came out last week to inspect it. The inspector said when he's seen this in the past Blaze King will send a new stove out because they don't recommend on-premise welding holding up to firebox temperatures. He also said the where the crack is the weld looked thin or not deep enough (sorry don't know welding terminology). You can see a difference in the weld where the crack occurred... it doesn't look as "full" as the rest of the weld.

The dealer just got back to me and said they contacted Blaze King and I am out of warranty by 2-3 months, so they can't do anything for me. My stove was installed February, 2018. I store my wood in a wood shed and it's always around 15% moisture. The catalyst is in good shape and I get an annual stove and chimney cleaning/inspection from the dealer. I'm not sure what else I can do as a responsible wood stove owner.

Is there anything you guys can recommend? I am 100% not satisfied with my dealers or Blaze King's response.

[Hearth.com] Weld Crack in Blaze King Princess
 
100% I'd reweld that onsite.

Grind it completely out, weld it with 7018 stick. Clean it up and repaint the area.

If you were my neighbour I'd fix that for a 12 pack, wouldn't take more than an hour.

@BKVP do you have a different opinion?
Well, I wish you were my neighbor. Heck, I'd give you a 30-pack!
 
  • Like
Reactions: ABMax24
That should be on-site repairable by a competent welder.
 
  • Like
Reactions: Tar12
That should be on-site repairable by a competent welder.
Easily repairable...that repair is childs play for a good welder..
 
Where does the door seal? Around that flange, or does the flange itself go into the door?
 
That rim presses in the gasket on the door
 
  • Like
Reactions: TomMcDonald
Bk will come through. Had this been 20 year old stove……
 
100% I'd reweld that onsite.

Grind it completely out, weld it with 7018 stick. Clean it up and repaint the area.

If you were my neighbour I'd fix that for a 12 pack, wouldn't take more than an hour.

@BKVP do you have a different opinion?
Will 7018 stick hold up to the hot temperature in a firebox?
 
100% I'd reweld that onsite.

Grind it completely out, weld it with 7018 stick. Clean it up and repaint the area.

If you were my neighbour I'd fix that for a 12 pack, wouldn't take more than an hour.

@BKVP do you have a different opinion?
I asked, because I just got my firebox welded with 7018 electron
 
7018 will stick just fine and should be stronger than the base metal. Not many folks still burn rods though.
 
  • Like
Reactions: Itslay90
Bk will come through. Had this been 20 year old stove……
I discovered a 3" long crack in a weld on my Blaze King Princess at the end of burning season (March, 2023). I called my dealer who installed it and they came out last week to inspect it. The inspector said when he's seen this in the past Blaze King will send a new stove out because they don't recommend on-premise welding holding up to firebox temperatures. He also said the where the crack is the weld looked thin or not deep enough (sorry don't know welding terminology). You can see a difference in the weld where the crack occurred... it doesn't look as "full" as the rest of the weld.

The dealer just got back to me and said they contacted Blaze King and I am out of warranty by 2-3 months, so they can't do anything for me. My stove was installed February, 2018. I store my wood in a wood shed and it's always around 15% moisture. The catalyst is in good shape and I get an annual stove and chimney cleaning/inspection from the dealer. I'm not sure what else I can do as a responsible wood stove owner.

Is there anything you guys can recommend? I am 100% not satisfied with my dealers or Blaze King's response.

View attachment 312568
Whatever happened? Did you get it fixed?
 
Not certain about details. When we see this, typically it is from an air leak. Usually owners are honest and say they've never adjusted the door or replaced a gasket.

It is very repairable. Drill 1/8" hole at each end to terminate the crack, then grind, weld and paint.

Also, lastly, 2-3 months out of warranty would have crossed my desk but I don't recall this at all.

BKVP
 
  • Like
Reactions: Tron and Itslay90